PPS is a high-temperature engineering plastic with high rigidity, low water absorption, and narrow processing window. It requires strict control of drying, temperature, injection, and cooling to avoid
2026/02/28 Injection Molding
TPR is a thermoplastic elastomer with medium fluidity and low corrosion. Mold steel selection depends on hardness, transparency, output, and appearance requirements.Key Requirements for TPR MoldsWear
2026/02/28 Injection Molds
TPE (thermoplastic elastomer) offers soft touch, elasticity, and good processability, widely used in consumer goods, handles, electronics, automotive, and sealing components. TPE compounds often conta
2026/02/27 Injection Molding
Insufficient clamping force causes flash, overflow, oversized parts, and mold damage. Many flash issues are mistakenly solved by increasing clamping force without identifying the real cause. This arti
2026/02/27 Injection Moldshooren
TPU (Thermoplastic Polyurethane) is a widely used elastomer with high melt viscosity, poor flowability, strong tendency to adhere to mold surfaces, and slight corrosiveness when exposed to high temper
2026/02/26 Injection Molds
Mold temperature controllers, also known as mold heaters or chillers, are key equipment in injection molding. They stabilize mold surface temperature, directly affecting cooling rate, crystallinity, i
2026/02/24 Injection Mold
P20 steel (GB 3Cr2Mo, WNr 2311) is the most widely used pre-hardened plastic mold steel. It offers good machinability, polishing performance, and toughness with factory hardness HRC 30–36. It is widel
2026/02/24 Injection Molding
Flash, also called burrs or overflow, is a common defect in injection molding where molten plastic escapes from the parting line, ejector pins, inserts, or vents. Flash not only increases trimming lab